The floor had severe cracking and sanding issues, and the repair was completed using four Bonddex products.

Before repair, the cracks on the floor were pre-treated with a shot blasting machine, followed by cleaning and application of ARC-76 for bonding old and new surfaces. R-1 cement was then applied to fill the cracks.

After drying, CPP Primer was applied, followed by CPP Topcoat after crystallization to complete the repair process.